Standard Inspection Bureau clarified about the media coverage of the national standard of coated lea

The 2017, 12 August 1997 Storm

media national standards of coated lead content Cf. China "low", standard inspection bureau clarified response as follows:

1.Standard inspection agency coatings lead content provisions with reference to the European Union (soluble lead content 90 ppm), Japan (total lead content below 600 ppm, 90 ppm soluble following developed countries such as the specification), the National Institute of Standards and Technology (such as the Commission invited outputs Coatings Association), Officer (such as the Environmental Protection Department), study and research (such as building research institute of the Ministry of the Interior) and green groups caretaker Taiwan Association, study, CARETAKER Taiwan Association recommends room using coated to total lead content control, but the participants considered that the room using coated infant licking food to be soluble lead content control can be more consistent with the actual situation of the body was fully discussed and consensus from all walks of life, to 105 on 29 August Announcement of CNS 15931 "coated general safety requirement", the provisions of general consumer use indoor/outdoor and indoor use coated soluble lead content of 90 ppm, outdoor coated total lead content is below 600 ppm for industrial coatings is picking warning mark in order to avoid misuse of consumers. Other than 105 on 14 June revised publication CNS 12642 "Public children playground equipment", provided their material shall not contain hazardous substances such as lead for related units to follow.

2.Soluble lead content detection method to simulate drying coating and stamach after the Swallow role to detect in the body of its actual soluble output with the lead content in toys test law, mainly to avoid similar children. The coated elements in major advanced countries to test precision instruments such as atomic-optical scanner, Inductive coupled plasma atomic emission spectrometer for quantitative analysis. X-Ray Fluorescence Spectrometer (XRF) Because Precision Low only canbe used as paint dry film for initial detection screening, States have not yet XRF listed as Standard Test Method, standard inspection bureau will depend on the future technology development, timely XRF into detection criteria.
3.Standard inspection bureau has been commonly used in consumer coatings such as CNS 4940 "water-cement paint (latex paint)" and children's toys, the lead content in the exam should be applied to maintain the child safety.

4.Coatings lead content mainly industrial steel components such as brige etc.) of corrosion and corrosion problems as a result of involving the use of security that does not currently have a comprehensive ban on States, but to encourage the adoption of low lead coating and substitute products such as CNS 15667 "lead free no chrome anti-corrosion coatings".
5.The current world coatings lead content, States not yet consistent (total lead content 90 ppm~1000 ppm), the following are the existing CNS 15931 "coated general safety requirement" from harmful heavy metals such as lead content control values consistent with the EU and Japan, but the industry considered that can continue to gradual adjustment, standard inspection bureau will continue to collect relevant information among international and domestic production and use of a meeting on the status of study related issues and outputs, officer, study and research community consensus and timely review Revision. (Economy Standard Inspection Bureau) Date:2017-08-14

Share to